The Subject Of The Contract Is The Service Of Making A Refractory Kpo1 Rotary And Scaled Furnace, Intended For The Production Of Metal Oxides. The Process Of Obtaining Metal Oxides Is Carried Out In The Process Of Oxidizing Solid Raw Materials In The Form Of Crushed Minerals, Small Scrap Metal Or Metallic Powders, And In The Process Of Drying Concentrates Containing Up To 40% Humidity. The Temperature Range Of Operations Is From Around 300 ° C To About 800 ° C. Cubstilation In The Form Of A Formed High -Quality Refractory Material, With Parameters As Below: • Chemical Composition: From 58.5% To 60.5% Al2o3, From 1.8% To 2.0% Fe2o3 • Shepical Density: From 2.25 G/Cm3 To 2.40 G/Cm3 • Temperature Resistance: 1600 °. Swz.